PTFE vs PEEK vs POM: Which Engineering Plastic Should You Specify?

These three are the workhorses of custom non-metallic machining, and they are also the three most commonly confused. All are machinable, all are available as rod and plate, and all can be supplied in natural, black or filled grades. The differences show up the moment the part meets heat, load or a chemical.

The short version

  • POM (acetal, Delrin) — the default for mechanical parts. Stiff, dimensionally stable, machined easily, cheapest of the three. Fails above roughly 100 °C in continuous service and does not like strong acids.
  • PTFE (Teflon) — the chemical and low-friction specialist. Works from cryogenic temperatures to about 260 °C and resists nearly every chemical. Soft, and it creeps under sustained load, so it needs a filler grade when it carries a force.
  • PEEK — the high-performance choice. Holds strength past 250 °C, survives steam and autoclaving, and has excellent wear resistance and purity. It costs several times what PTFE or POM cost, so it should be specified for a reason.

Temperature

Continuous service temperature is usually the fastest way to separate them. POM is comfortable to about 90–100 °C. PTFE sits at 260 °C. PEEK holds useful mechanical strength to 250 °C and can be autoclaved repeatedly, which is why medical and semiconductor parts gravitate to it.

If your maximum working temperature is under 90 °C, specifying PEEK is paying for a capability you will never use.

Chemical resistance

PTFE is the near-universal answer: it resists acids, bases, solvents and oxidisers across the whole pH range, with molten alkali metals and elemental fluorine as the standing exceptions. PEEK resists most acids and organics but is attacked by concentrated sulphuric acid and some halogenated solvents. POM is fine with fuels, oils, alcohols and neutral chemicals but degrades in strong acids and oxidising agents.

Sealing a hot aggressive chemical is a PTFE job, not a POM job, no matter what the price list says.

Wear and friction

PTFE has the lowest friction coefficient of any common plastic and is chosen for non-stick sliding contact. The catch is that it wears relatively fast under high load, so filled grades (glass, carbon, bronze) are used when a PTFE part must also carry load.

POM is the natural choice for dry-running gears and bushings: it has good fatigue resistance, holds its shape and machines to tight tolerance. PEEK and PEEK composite grades outperform both where the part also sees temperature, steam or heavy load.

Creep and dimensional stability

PTFE creeps under continuous load even at room temperature, so a PTFE gasket that is compressed permanently will lose sealing force over time. POM and PEEK are far more stable — POM barely moves with humidity, while nylon (the common alternative for bushings) grows noticeably.

For a press-fit bushing that must stay put, POM or PEEK beats PTFE. For a chemically exposed seal that gets re-torqued, PTFE is still right.

Cost

Cost runs roughly POM < PTFE < PEEK, with PEEK several times POM for the same blank size, and stocked filled or medical grades higher again. Because material is a large share of the price of a machined part, the choice has a direct effect on unit cost — so make the cheapest material that meets the real operating conditions the starting point, and only move up when temperature, chemistry, purity or wear rules it out.

Which one for which part

Part Best default Move up when
Chemical pump valve seat PTFE Pressure and load need a filled grade
Dry-running gear POM Temperature above 100 °C → PEEK
Bushing, press fit POM High temperature or steam → PEEK
Semiconductor insulator PEEK —
Low-friction wear strip PTFE Load-bearing → filled PTFE
Food-contact roller POM (FDA grade) Steam or CIP at high temperature → PEEK

Next step

Every one of these materials has a full ten-section selection guide on this site — properties, machining notes, stock forms and an FAQ:

PTFE · PEEK · POM · all materials compared

Still undecided? Send the drawing with the operating temperature, the medium and the load, and we will recommend a grade rather than quote the cheapest one on the shelf. Request a quote.