Most specification mistakes we see are not exotic. They are a PTFE part asked to carry a load it creeps under, a nylon bushing that swells in humidity and seizes, a standard EPDM gasket pushed past 150°C, or a PEEK seal specified where PVC would have done the same job for a fraction of the price.
The table below is the decision shortcut we use internally. Every material name links to its full ten-section selection guide, where you will find typical property values, machining notes, stock forms, and a fit / does-not-fit list.
| Material | Watch out for | Cost | Full guide |
|---|---|---|---|
| PTFE | Cold flow under load; needs filling for pressure | High | PTFE |
| PEEK | Cost; needs a real reason (temperature, purity, steam) | Very high | PEEK |
| POM (Acetal / Delrin) | Nothing above ~100°C or in strong acids | Low | POM |
| Nylon (PA6 / PA66) | Moisture growth changes dimensions; UV without stabiliser | Low–medium | Nylon |
| PVC (incl. CPVC) | Not for hot steam; limited mechanical load | Low | PVC |
| UHMWPE | Creeps under sustained load; hard to glue | Low–medium | UHMWPE |
| Silicone (VMQ) | Tears easily; swells in many oils and fuels | Medium | Silicone |
| EPDM | Hydrocarbon oils and fuels destroy it | Low | EPDM |
| NBR (Nitrile) | Ozone, weathering and ketones; not for outdoor | Low | NBR |
| Polyurethane (PU) | Hydrolysis in hot wet service; limited to ~80–90°C | Medium | Polyurethane |
| Graphite | Brittle; dust needs handling; grade choice matters | Medium | Graphite |
| Ceramics (alumina, zirconia, SiC, Si₃N₄) | Brittle in tension; shrinkage must be allowed for | High | Ceramics |
| Carbon fibre (CFRP) | Cost; galvanic corrosion against metals; dust | High | Carbon Fibre |
| FRP / GRP | Lower stiffness than CFRP; resin choice drives chemicals | Low–medium | FRP |
How to use it
Start from the two constraints that usually decide the material — maximum continuous temperature and the medium it touches — then check wear mode and required tolerance. If two materials both pass, pick the cheaper one and note why on the drawing.
- Temperature above 150°C, steam, or autoclave → PEEK, ceramics or graphite.
- Aggressive chemicals across the whole pH range → PTFE (with a filler grade if under load).
- Quiet dry-running gears and precision mechanisms → POM, or nylon where shock load dominates.
- Hot water, weather and outdoor seals → EPDM, silicone or polyurethane.
- Wear strips, chute liners, low-friction sliding → UHMWPE, PTFE-filled POM.
- Electrical insulation with thermal stability → PEEK, ceramic, FRP/G10.
Related reading
Not sure which way to go? Send the drawing, the operating temperature and the medium, and we will recommend a grade rather than just quote the cheapest option. Request a quote.